Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese Celstran® PP-GF40-03-Black PP, 40% Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Celanese Corporation
Trade Name CELSTRAN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Celstran® PP-GF40-03-Black PP, 40% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% long glass fiber reinforced, chemically coupled, heat stabilized, Polypropylene BLACKInformation provided by Celanese
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
5mm/min; ISO 527-2/1A
Elongation at Break 2.00 %
2.00 %
5mm/min; ISO 527-2/1A
Tensile Modulus 8.70 GPa
1260 ksi
50mm/min; ISO 527-2/1A
Flexural Strength 190 MPa
27600 psi
ISO 178
Flexural Modulus 8.40 GPa
1220 ksi
ISO 178
Charpy Impact, Notched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Processing Temperature 40.0 - 70.0 °C
104 - 158 °F
cavity
Feed Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Zone 1 210 - 220 °C
410 - 428 °F
Zone 2 220 - 230 °C
428 - 446 °F
Zone 3 230 - 240 °C
446 - 464 °F
Zone 4 230 - 250 °C
446 - 482 °F
Die Temperature 230 - 250 °C
446 - 482 °F
Melt Temperature 230 - 250 °C
446 - 482 °F
Drying Temperature 90.0 - 100 °C
194 - 212 °F
Dry Time 2.00 hour
2.00 hour
Moisture Content <= 0.200 %
<= 0.200 %
Descriptive Properties Value Comments
Injection molding Yes