Celanese Celstran® PA66-GF50-02 P11 Nylon 66, 50% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Celanese Corporation
Trade Name CELSTRAN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Celstran® PA66-GF50-02 P11 Nylon 66, 50% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material code according to ISO 1043-1: PA66Information provided by Celanese
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 260 MPa
37700 psi
5mm/min; ISO 527-2/1A
Elongation at Break 2.20 %
2.20 %
5mm/min; ISO 527-2/1A
Tensile Modulus 16.4 GPa
2380 ksi
50mm/min; ISO 527-2/1A
Flexural Strength 425 MPa
61600 psi
ISO 178
Flexural Modulus 14.85 GPa
2154 ksi
ISO 178
Charpy Impact, Notched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1,-2,-3