Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese Celstran® PA6-GF40-01 Nylon 6, 40% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer Celanese Corporation
Trade Name CELSTRAN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Celstran® PA6-GF40-01 Nylon 6, 40% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% long strand glass fiber reinforced nylon 6 NaturalInformation provided by Celanese
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.000500 - 0.00100 cm/cm
0.000500 - 0.00100 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.00250 - 0.00300 cm/cm
0.00250 - 0.00300 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 205 MPa
29700 psi
5mm/min; ISO 527-2/1A
237 MPa
34400 psi
ASTM D638
106 MPa

@Temperature 121 °C
15400 psi

@Temperature 250 °F
ASTM D638
281 MPa

@Temperature -40.0 °C
40800 psi

@Temperature -40.0 °F
ASTM D638
Elongation at Break 2.11 %
2.11 %
5mm/min; ISO 527-2/1A
2.50 %
2.50 %
ASTM D638
2.60 %

@Temperature 4.44 °C
2.60 %

@Temperature 40.0 °F
ASTM D638
3.00 %

@Temperature 121 °C
3.00 %

@Temperature 250 °F
ASTM D638
Tensile Modulus 12.4 GPa
1800 ksi
50mm/min; ISO 527-2/1A
13.4 GPa
1950 ksi
ASTM D638
7.31 GPa

@Temperature 121 °C
1060 ksi

@Temperature 250 °F
ASTM D638
11.8 GPa

@Temperature -40.0 °C
1710 ksi

@Temperature -40.0 °F
ASTM D638
Flexural Strength 335 MPa
48600 psi
ISO 178
339 MPa
49100 psi
ASTM D790
159 MPa

@Temperature 121 °C
23000 psi

@Temperature 250 °F
ASTM D790
398.2 MPa

@Temperature -40.0 °C
57750 psi

@Temperature -40.0 °F
ASTM D790
Flexural Modulus 11.15 GPa
1617 ksi
ISO 178
11.8 GPa
1710 ksi
ASTM D790
6.07 GPa

@Temperature 121 °C
880 ksi

@Temperature 250 °F
ASTM D790
12.5 GPa

@Temperature -40.0 °C
1810 ksi

@Temperature -40.0 °F
ASTM D790
Izod Impact, Notched 3.68 J/cm
6.90 ft-lb/in
ASTM D256
3.04 J/cm

@Temperature -40.0 °C
5.70 ft-lb/in

@Temperature -40.0 °F
ASTM D256
5.13 J/cm

@Temperature 121 °C
9.60 ft-lb/in

@Temperature 250 °F
ASTM D256
Charpy Impact, Notched 3.20 J/cm²
15.2 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1, -2
210 °C
410 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 80.0 - 100 °C
176 - 212 °F
cavity
Feed Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Middle Barrel Temperature 70.0 - 80.0 °C
158 - 176 °F
Zone 1 265 - 275 °C
509 - 527 °F
Zone 2 270 - 275 °C
518 - 527 °F
Zone 3 275 - 280 °C
527 - 536 °F
Zone 4 275 - 280 °C
527 - 536 °F
Die Temperature 275 - 280 °C
527 - 536 °F
Melt Temperature 270 - 280 °C
518 - 536 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Moisture Content <= 0.180 %
<= 0.180 %
Descriptive Properties Value Comments
Injection molding Yes
Copyright © lookpolymers.com All Rights Reserved