Material Notes:
Description: Celcon WR25HT is a black, weather resistant, tough acetal copolymer formulated for very high impact properties, It has high melt strength for extrusion and blow molding applications, while still being injection moldable.Information provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.0 MPa
5370 psi
50 mm/min; ISO 527-2/1A
Tensile Modulus 1.22 GPa
177 ksi
1 mm/min; ISO 527-2/1A
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched (ISO) 11.8 kJ/m²
5.61 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
ISO 75-1, -2
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
Mold Temperature 77.0 - 93.0 °C
171 - 199 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 3 hour
3 hour
Injection Pressure 75.8 - 110 MPa
11000 - 16000 psi