Material Notes:
Description: Celcon MT24U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Celcon MT24U01 is a low melt viscosity for fast cycling, thin walled injection molding.Information provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183 & ASTM D792
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 66.0 MPa
9570 psi
50 mm/min; ISO 527-2/1A
Flexural Modulus 2.75 GPa
399 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
ISO 75-1, -2
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
Mold Temperature 77.0 - 93.0 °C
171 - 199 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 3 hour
3 hour
Injection Pressure 75.8 - 110 MPa
11000 - 16000 psi