Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese Celanex® 5300-2UV PBT, 30% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Celanese Corporation
Trade Name Celanex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Celanex® 5300-2UV PBT, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Celanese Corporation.
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
50mm/min; ISO 527-2/1A
Elongation at Break 2.0 %
2.0 %
50mm/min; ISO 527-2/1A
Tensile Modulus 9.20 GPa
1330 ksi
1mm/min; ISO 527-2/1A
Charpy Impact, Notched 0.560 J/cm²
2.66 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Processing Temperature 20.0 - 50.0 °C
68.0 - 122 °F
hopper
65.0 - 93.0 °C
149 - 199 °F
cavity
Feed Temperature 230 - 250 °C
446 - 482 °F
Zone 1 230 - 250 °C
446 - 482 °F
Zone 2 235 - 255 °C
455 - 491 °F
Zone 3 235 - 255 °C
455 - 491 °F
Zone 4 240 - 260 °C
464 - 500 °F
Die Temperature 250 - 265 °C
482 - 509 °F
Melt Temperature 235 - 265 °C
455 - 509 °F
Hot-Working Temperature 250 - 260 °C
482 - 500 °F