Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese Celanex® 2000 Polyester (PBT)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer Celanese Corporation
Trade Name Celanex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Celanex® 2000 Polyester (PBT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High melt flowInformation provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 0.090 %
0.090 %
ASTM D570
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ISO 2039-2
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 85.0 MPa
12300 psi
ISO 178
Flexural Modulus 2.60 GPa
377 ksi
ISO 178
Izod Impact, Notched (ISO) 3.20 kJ/m²
1.52 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
UL94
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.2

@Frequency 100 Hz
3.2

@Frequency 100 Hz
Dielectric Strength 17.0 kV/mm

@Thickness 3.17 mm
432 kV/in

@Thickness 0.125 in
50% R.H.; ASTM D149
Dissipation Factor 0.0020

@Frequency 100 Hz
0.0020

@Frequency 100 Hz
Comparative Tracking Index >= 600 V
>= 600 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved