Celanese CELANEX 3300-2LM PBT, Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
Manufacturer Celanese Corporation
Trade Name CELANEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese CELANEX 3300-2LM PBT, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release. It is a lasermarkable grade available in a black color to mark white, The grade is specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating in the UV region (355nm) may yield different resultsInformation provided by Celanese
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90.0
90.0
ISO 2039-2
Tensile Strength at Break 130 MPa
18900 psi
5mm/min; ISO 527-2/1A
134 MPa
19500 psi
ASTM D638
Elongation at Break 2.00 %
2.00 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
210 MPa
30500 psi
ISO 178
Flexural Modulus 9.70 GPa
1410 ksi
ISO 178
82.7 GPa
12000 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 7.50 kJ/m²
3.57 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
403 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
250 - 260 °C
482 - 500 °F
hot runner
Feed Temperature 230 - 240 °C
446 - 464 °F
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Zone 1 230 - 240 °C
446 - 464 °F
Zone 2 235 - 250 °C
455 - 482 °F
Zone 3 235 - 250 °C
455 - 482 °F
Zone 4 240 - 260 °C
464 - 500 °F
Die Temperature 250 - 260 °C
482 - 500 °F
Melt Temperature 235 - 260 °C
455 - 500 °F