Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.954 - 0.956 g/cc | 0.954 - 0.956 g/cc | DIN 51 757, Method D |
Density | 0.00616 g/cc | 0.000223 lb/in³ | Vapor density |
Water Absorption | 4.0 % | 4.0 % | |
Solubility in Water | 3.0 % | 3.0 % | |
Viscosity | 0.71 cP @Temperature 20.0 °C |
0.71 cP @Temperature 68.0 °F |
|
Molecular Weight | 146.19 g/mol | 146.19 g/mol | |
Vapor Pressure | 0.000340 bar @Temperature 20.0 °C |
0.255 torr @Temperature 68.0 °F |
|
Storage Temperature | 18.3 - 37.8 °C | 64.9 - 100 °F |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 318.4 J/g @Pressure 0.101 MPa |
137.0 BTU/lb @Pressure 14.7 psi |
|
Specific Heat Capacity | 1.93 J/g-°C | 0.461 BTU/lb-°F | |
Melting Point | -80.0 °C | -112 °F | |
Boiling Point | 170 °C @Pressure 0.101 MPa |
338 °F @Pressure 14.7 psi |
|
Flash Point | 68.0 °C | 154 °F | DIN EN ISO 2719 |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.408 - 1.41 @Temperature 20.0 °C |
1.408 - 1.41 @Temperature 68.0 °F |
n<sub>D</sub>; DIN 51 423, part 2 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.25e+8 ohm-cm | 1.25e+8 ohm-cm | |
Dielectric Constant | 8.0 | 8.0 |
Descriptive Properties | Value | Comments |
---|---|---|
Evaporation Number | 57 | DIN 53 170; diethyl ether = 1 |