Celanese Ateva® 1985A Ethylene Vinyl Acetate Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Ateva® 1985A Ethylene Vinyl Acetate Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ateva® 1985A resin is suitable for use in hot melt glue stick adhesive applications. It contains an antioxidant to minimize viscosity changes of the hot melt blends during processing. It complies with Code of Federal Regulation 21 CFR Section 177.1350 and 175.105, subject to extraction limitations for specific end use applications. Additives: AntioxidantApplications: Adhesives & SealantsInformation provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 0.931 g/cc
0.0336 lb/in³
ASTM D1505; ASTM D1928 Proc A
Vinyl Acetate Content 19 %
19 %
AT Plastics PTM-39
Melt Flow 600 g/10 min

@Load 0.325 kg,
Temperature 125 °C
600 g/10 min

@Load 0.716 lb,
Temperature 257 °F
Modified; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength at Break 3.50 MPa
508 psi
Type IV (50 mm/min); ASTM D638
Elongation at Break 540 %
540 %
Type IV (50 mm/min); ASTM D638
Flexural Modulus 0.0260 GPa
3.77 ksi
1% Secant; ASTM D790
Thermal Properties Metric English Comments
Ring & Ball Softening Point 87.0 °C
189 °F
ASTM E28