Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese 50000446 Methyl Isobutyl Ketone (MIBK)

Category Fluid , Solvent
Manufacturer Celanese Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese 50000446 Methyl Isobutyl Ketone (MIBK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CAS Number: 108-10-1Methyl Isobutyl Ketone (MIBK) is a colorless liquid exhibiting a faint ketonic and camphor-like odor. One of the most useful among the acetone derivate solvents, it has a medium evaporation rate. MIBK is stable and does not polymerize. MIBK is highly compatible with a variety of organic reagents and is a good solvent for a wide range of industrial materials..Possible applications: End uses for MIBK include coating solvents, rare-metal extraction, process solvent for adhesives, ink formulations, leather finishing, pharmaceuticals, and as a chemical intermediate. MIBK is an excellent solvent for cellulose-based and resin-based coating systems. It is a useful solvent for pyrethrins, rubber cements and model dopes. It is a chemical intermediate for rubber antioxidants and specialty surfactants. MIBK contains dewaxing and separating properties, which can be used in the purification of different chemicals, mineral oils, tall oil, stearic acid and butanol.Information provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 0.00427 g/cc
0.000154 lb/in³
Vapor density
0.7734 g/cc

@Temperature 50.0 °C
0.02794 lb/in³

@Temperature 122 °F
0.7781 g/cc

@Temperature 45.0 °C
0.02811 lb/in³

@Temperature 113 °F
0.7827 g/cc

@Temperature 40.0 °C
0.02828 lb/in³

@Temperature 104 °F
0.7872 g/cc

@Temperature 35.0 °C
0.02844 lb/in³

@Temperature 95.0 °F
0.7918 g/cc

@Temperature 30.0 °C
0.02861 lb/in³

@Temperature 86.0 °F
0.7963 g/cc

@Temperature 35.0 °C
0.02877 lb/in³

@Temperature 95.0 °F
0.8007 g/cc

@Temperature 20.0 °C
0.02893 lb/in³

@Temperature 68.0 °F
0.8052 g/cc

@Temperature 15.0 °C
0.02909 lb/in³

@Temperature 59.0 °F
0.8096 g/cc

@Temperature 10.0 °C
0.02925 lb/in³

@Temperature 50.0 °F
0.8139 g/cc

@Temperature 5.00 °C
0.02940 lb/in³

@Temperature 41.0 °F
0.8183 g/cc

@Temperature 0.000 °C
0.02956 lb/in³

@Temperature 32.0 °F
Solubility in Water 1.9 %
1.9 %
Viscosity 0.40 cP

@Temperature 50.0 °C
0.40 cP

@Temperature 122 °F
0.51 cP

@Temperature 30.0 °C
0.51 cP

@Temperature 86.0 °F
0.58 cP

@Temperature 20.0 °C
0.58 cP

@Temperature 68.0 °F
Molecular Weight 100.16 g/mol
100.16 g/mol
Vapor Pressure 0.00560 bar

@Temperature 0.000 °C
4.20 torr

@Temperature 32.0 °F
0.00790 bar

@Temperature 5.00 °C
5.93 torr

@Temperature 41.0 °F
0.0109 bar

@Temperature 10.0 °C
8.18 torr

@Temperature 50.0 °F
0.0148 bar

@Temperature 15.0 °C
11.1 torr

@Temperature 59.0 °F
0.0200 bar

@Temperature 20.0 °C
15.0 torr

@Temperature 68.0 °F
0.0265 bar

@Temperature 25.0 °C
19.9 torr

@Temperature 77.0 °F
0.0348 bar

@Temperature 30.0 °C
26.1 torr

@Temperature 86.0 °F
0.0452 bar

@Temperature 35.0 °C
33.9 torr

@Temperature 95.0 °F
0.0581 bar

@Temperature 40.0 °C
43.6 torr

@Temperature 104 °F
0.0740 bar

@Temperature 45.0 °C
55.5 torr

@Temperature 113 °F
0.0934 bar

@Temperature 50.0 °C
70.1 torr

@Temperature 122 °F
Surface Tension 20.8 dynes/cm

@Temperature 50.0 °C
20.8 dynes/cm

@Temperature 122 °F
22.9 dynes/cm

@Temperature 30.0 °C
22.9 dynes/cm

@Temperature 86.0 °F
24 dynes/cm

@Temperature 20.0 °C
24 dynes/cm

@Temperature 68.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 391 J/g

@Temperature 50.0 °C
168 BTU/lb

@Temperature 122 °F
403 J/g

@Temperature 30.0 °C
173 BTU/lb

@Temperature 86.0 °F
409 J/g

@Temperature 20.0 °C
176 BTU/lb

@Temperature 68.0 °F
Specific Heat Capacity 2.12 J/g-°C

@Temperature 20.0 °C
0.507 BTU/lb-°F

@Temperature 68.0 °F
2.15 J/g-°C

@Temperature 30.0 °C
0.514 BTU/lb-°F

@Temperature 86.0 °F
2.21 J/g-°C

@Temperature 50.0 °C
0.528 BTU/lb-°F

@Temperature 122 °F
Thermal Conductivity 0.137 W/m-K

@Temperature 50.0 °C
0.951 BTU-in/hr-ft²-°F

@Temperature 122 °F
0.143 W/m-K

@Temperature 30.0 °C
0.992 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
0.145 W/m-K

@Temperature 20.0 °C
1.01 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Melting Point >= -84.0 °C
>= -119 °F
Boiling Point 116 °C

@Pressure 0.101 MPa
241 °F

@Pressure 14.7 psi
Flash Point 16.0 °C
60.8 °F
Optical Properties Metric English Comments
Refractive Index 1.3958

@Temperature 20.0 °C
1.3958

@Temperature 68.0 °F
n<sub>D</sub>; DIN 51 423
Chemical Properties Metric English Comments
Critical Pressure 32.7 bar
24500 torr
Critical Temperature 301.5 °C
574.7 °F
Descriptive Properties Value Comments
Evaporation Rate 5.6
(n-Butyl Acetate =1)
Copyright © lookpolymers.com All Rights Reserved