Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese 192 LDPE polymer for adhesives, automotive and compounds

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Celanese Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese 192 LDPE polymer for adhesives, automotive and compounds.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
192 is a homopolymer that is suitable for use in carpet extrusion coating applications. This polymer may be processed on conventional extrusion coating equipment. Additives: Applications: AutomotiveInformation provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 0.9125 g/cc
0.03297 lb/in³
AT Plastics PTM-03
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength at Break 8.00 MPa
1160 psi
Type IV (50 mm/min); ASTM D638
Elongation at Break 100 %
100 %
Type IV (50 mm/min); ASTM D638
Flexural Modulus 0.160 GPa
23.2 ksi
1% Secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
DSC; ASTM D3417
Vicat Softening Point 71.2 °C
160 °F
ASTM D1525
Brittleness Temperature -10.0 °C
14.0 °F
ASTM D746
Copyright © lookpolymers.com All Rights Reserved