Carmel Olefins CARMELCOAT™ MT 34 EC Specialty Polypropylene for Extrusion Coating

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Carmel Olefins
Trade Name CARMELCOAT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CARMELCOAT™ MT 34 EC Specialty Polypropylene for Extrusion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CARMELCOAT™ MT 34 EC is a specialty polypropylene developed for extrusion coating and lamination. This grade exhibits improved process ability for applications which requires high coating speeds, low coating weight, low neck-in, good adhesion to substrate and high temperature resistance. APPLICATIONS CARMELCOAT ™ MT 34 EC is suitable for extrusion coating and lamination of paper, paperboards, plastic film, woven PP cloths, and PP based nonwoven fabrics.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D1505
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus 1.025 GPa
148.7 ksi
ASTM D790
Izod Impact, Notched 0.230 J/cm

@Temperature >=23.0 °C
0.431 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 132 °C

@Load 1.02 kg
270 °F

@Load 2.25 lb
ASTM D1525
Processing Properties Metric English Comments
Die Temperature 310 °C
590 °F
Melt Temperature 280 - 330 °C
536 - 626 °F