Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carmel Olefins CAPILENE® U 77 AV Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® U 77 AV Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CAPILENE® U 77 AV is a high melt flow rate polypropylene homopolymer controlled rheology, designed for injection molding of products with long flow length. It is specially formulated with antistatic and nucleating additives, allowing fast cycle due to high de-molding temperature and reducing cooling time. It exhibits high stiffness combined with high flow ability and good contact clarity. APPLICATIONS CAPILENE ® U 77 AV is designed for multi-cavity injection molding, thin walled packaging items, products with long flow length, household articles and toys.
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.75 GPa
254 ksi
ASTM D790
Izod Impact, Notched 0.250 J/cm

@Temperature >=23.0 °C
0.468 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM D1525