Carmel Olefins CAPILENE® U 77 A Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® U 77 A Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® U 77 A is a high melt flow rate homopolymer for injection molding of products with long flow length. It is specially formulated with antistatic and nucleating additives, allowing fast cycle due to high de-molding temperature and reduced cooling time. It exhibits high stiffness combined with high flowability and good contact clarity.Applications: CAPILENE® U 77 A is designed for multi-cavity injection molding, thin walled packaging items, products with long flow length, household articles and toys. In comparison to CAPILENE® U 77 AV it offers a better choice for food packaging containers.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
50 mm/min; ASTM D638
Elongation at Yield 11 %
11 %
50 mm/min; ASTM D638
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM D1525