Material Notes:
Description: CAPILENE® QT 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QT 73 AV is clarified with antistatic additivation. It exhibits good flowability combined with good impact strength at ambient temperature, low warpage and high transparency.Applications: CAPILENE® QT 73 AV is suitable for injection molding of transparent thin wall items, clarified food containers and household articles.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ASTM D638
Elongation at Yield 14 %
14 %
50 mm/min; ASTM D638
Flexural Modulus 1.05 GPa
152 ksi
ASTM D790
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 130 °C

@Load 1.02 kg
266 °F

@Load 2.25 lb
ASTM D1525
Optical Properties Metric English Comments
Haze 8.0 %

@Thickness 1.00 mm
8.0 %

@Thickness 0.0394 in
ASTM D1003
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 210 - 260 °C
410 - 500 °F
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F