Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carmel Olefins CAPILENE® M 45 F Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® M 45 F Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CAPILENE® M 45 F is a polypropylene homopolymer developed for the production of cast films. It is formulated with slip and anti-blocking agents. They show high gloss, high transparency and good stiffness. APPLICATIONS CAPILENE ® M 45 F is suitable for cast unoriented films on chill roll extrusion, for blown unoriented water-quenched films extrusion, and for blown molding and injection molding products.
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm

@Temperature >=23.0 °C
0.562 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb
ASTM D1525
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
ASTM D1003