Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carmel Olefins CAPILENE® G 70 TF Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® G 70 TF Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® G 70 TF is a nucleated polypropylene homopolymer intended for sheet extrusion and thermoforming applications. This grade exhibits high stiffness, high gloss, good contact transparency, short cycle time and improved characteristics at high temperature.Applications: CAPILENE® G 70 TF is suitable for extrusion-thermoforming of thin, stiff and transparent food containers, containers for higher temperature filling.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
50 mm/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
50 mm/min; ASTM D638
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
ASTM D648
Vicat Softening Point 159 °C

@Load 1.02 kg
318 °F

@Load 2.25 lb
ASTM D1525
Optical Properties Metric English Comments
Haze 30 %

@Thickness 1.00 mm
30 %

@Thickness 0.0394 in
ASTM D1003
Transmission, Visible 90 %
90 %
transparent; thickness not quantified