Carmel Olefins CAPILENE® G 65 F Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® G 65 F Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® G 65 F is a polypropylene homopolymer designed for the production of biaxially oriented polypropylene films (BOPP). It exhibits good processability, easy film stretchability and good mechanical properties.Applications: Typical applications for CAPILENE® G 65 F are BOPP plain or coextruded packaging films. It doesn't contain slip or antiblock additives and is also calcium stearate free, therefore it is suitable for production of metallizable BOPP film.CAPILENE® G 65 F is also used with the extrusion and coextrusion thermoforming process were melt strength is of importance.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa
4790 psi
50 mm/min; ASTM D638
Elongation at Yield 15 %
15 %
50 mm/min; ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM D1525