Cadi Cu-Tungsten (80%) Copper Alloy

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Cadi Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cadi Cu-Tungsten (80%) Copper Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Slightly higher tungsten content results in higher hardness and strength when forces are relatively high. Strength is gained with a slight decrease in electrical and thermal properties.Information provided by Cadi Company.
Physical Properties Metric English Comments
Density 15.6 g/cc
0.563 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B >= 98

@Diameter <=25.4 mm
>= 98

@Diameter <=1.00 in
Component Elements Properties Metric English Comments
Copper, Cu 20 %
20 %
Tungsten, W 80 %
80 %
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.00000493 ohm-cm
<= 0.00000493 ohm-cm
Calculated from Min 35 %IACS
Descriptive Properties Value Comments
RMWA Class 12