Cadi C10100 Oxygen Free Copper

Category Metal , Nonferrous Metal , Copper Alloy , Wrought Copper , Pure Element
Manufacturer Cadi Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cadi C10100 Oxygen Free Copper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oxygen Free Copper is specified when resistance to hydrogen embrittlement is required due to application in a high temperature, hydrogen environment.Forms: RodBarPlateInformation provided by Cadi Company.
Physical Properties Metric English Comments
Density 8.94 g/cc
0.323 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F >= 80

@Diameter <=25.4 mm
>= 80

@Diameter <=1.00 in
hard temper
Component Elements Properties Metric English Comments
Copper, Cu >= 99.99 %
>= 99.99 %
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.00000176 ohm-cm
<= 0.00000176 ohm-cm
Calculated from Min 98 %IACS