CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer CPC - Vycom Co.
Trade Name VINTEC® II
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or where the finished product is subject to shock or physical abuse. Vintec II conforms to ASTM-D-1784-95 Class 16444-D (Formerly Type II Grade 1) and is manufactured without fillers or plasticizers. Its high heat deflection temperature and high modulus make it ideally suited for operation at temperatures up to 140º F with fewer supports than other Type II materials. Material conforming to former Type II classification were only required to have an Izod impact of 18 per ASTM-D-256. This allows the sheet to be cold rolled into large diameter cylinders for exhaust systems. Exceptional fire ratings UL-94V-0 and flame spread under 20 per ASTM-E-84 also enhance its position in this application. Vintec II is available in numerous colors, finishes and sizes.FEATURES AND BENEFITS Strength- Vintec II is a high impact strength product; over 15 times the value of standard PVC. Chemical Resistance- Vintec II has good chemical resistance to acids, alkalis and fumes. Ductility- Vintec II can be cold rolled for duct and ventilation applications. Formability- Vintec II has excellent thermoforming and vacuum forming characteristics. Workability- Vintec II can be cold rolled, formed, cut, shaped and welded. Consistency- Vintec II is extruded through its available range of gauges for dimensional consistency. Flammability- Vintec Ii is self extinguishing and it has a flame spread of 20 according to ASTM E84.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.16 %
0.16 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Tensile Modulus 2.73 GPa
396 ksi
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
Yeild; ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 20.0 °C
35.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 82.8 °C
181 °F
ASTM D1525
Flammability, UL94 V-0
V-0
Flame Spread Index 15
15
ASTM E84
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+15 ohm-cm
6.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.03

@Frequency 60 Hz
3.03

@Frequency 60 Hz
ASTM D150
Dielectric Strength 25.4 kV/mm
645 kV/in
ASTM D149
Dissipation Factor 0.0083

@Frequency 60 Hz
0.0083

@Frequency 60 Hz
ASTM D150
Dielectric Loss Index 0.025
0.025
ASTM D150
Descriptive Properties Value Comments
Chemical Resistance Class D
ASTM D1784
Flammability Self-Extinguishing
ASTM D635