Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CPC - Vycom FLAMETEC™ CP7-D Flame Retardant Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer CPC - Vycom Co.
Trade Name FLAMETEC™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom FLAMETEC™ CP7-D Flame Retardant Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flametec™ CP7-D is a proprietary designation for a flame retardant polypropylene formulation. CP7-D represent our version of polypropylene sheet whose flame retardant characteristics meet or exceed the most rigorous FMRC 4910 testing standards for most aspects of flame retardation, self-extinguishing characteristics and burnthrough. In addition, CP7-D also meets or exceeds test standards for low smoke generation and minimal toxic by-products. CP7-D is a filled PP sheet material, therefore, chemical compatibility should be verified for each application.FEATURES AND BENEFITS Impact Strength- Flexibility and strength of designs vs. other FRPP products. Weldability- Easy to fabricate with conventional welding equipment. Economics- An economical alternative for fire safe construction. Fire Safe- Listed in accordance to FMRC 4910, fire safe materials for clean room construction. Extruded Sheet- Offers the best gauge consistency, surface and tolerances.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
10 sec.; ASTM D785
Tensile Strength, Ultimate 17.2 MPa
2500 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 5.39 J/cm
10.1 ft-lb/in
1/8 in. notch; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Vicat Softening Point 148 °C
299 °F
1 kg; ASTM D1525
Flammability, UL94 5VA
5VA
ETL Labs
Flammability Test <= 0.010
<= 0.010
SDI, FMRC test data; File #3D7Q7.AM
<= 4.2
<= 4.2
FPI, FMRC test data; File #3D7Q7.AM
<= 25
<= 25
(flame) ETL Labs; ASTM E84 Tunnel Test
<= 100
<= 100
(smoke) ETL Labs; ASTM E84 Tunnel Test
Descriptive Properties Value Comments
Corner Weld Strength, lb/in 467
CPC Test