Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

C.O.I.M. LARIPUR® LPR6520 Standard Adipate Ester Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer , Polyurethane, TP
Manufacturer C.O.I.M. S.p.A.
Trade Name Laripur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. LARIPUR® LPR6520 Standard Adipate Ester Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGreat flexibility with constancy at temperature variationsGood compression resistanceGood water and light resistanceGood resistance to oils, fats and to many types of solventsSeries 20 Standard Adipate Ester: These products are based on saturated polyesters. They exhibit strength and durability with excellent tear and abrasion resistance; good hydrolytic stability resistance to solvents, oxidation and UV light degradation.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 64.7 MPa
9380 psi
ASTM D412
Elongation at Break 420 %
420 %
ASTM D412
50% Modulus 0.0195 GPa
2.83 ksi
ASTM D412
100% Modulus 0.0225 GPa
3.26 ksi
ASTM D412
300% Modulus 0.0440 GPa
6.38 ksi
ASTM D412
Flexural Modulus 0.360 GPa
52.2 ksi
ASTM D790
Tear Strength 190 kN/m
1080 pli
ASTM D624
Abrasion 40
40
mm3, Abrasion Loss; DIN 53516
Torsional Stiffness 77.0 MPa
11200 psi
+20°C; ASTM D1043
455 MPa
66000 psi
-20°C; ASTM D1043
Thermal Properties Metric English Comments
Vicat Softening Point 150 °C
302 °F
ASTM D1525