C.O.I.M. EXTER S® S 700 Self-extinguishing Resin

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer C.O.I.M. S.p.A.
Trade Name EXTER S®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. EXTER S® S 700 Self-extinguishing Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 700: Self-extinguishing resin for transparent laminates and corrugated sheetsInformation provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Brookfield Viscosity 120 - 180 cP

@Temperature 25.0 °C
120 - 180 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 72.0 °C
158 - 162 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Chemical Properties Metric English Comments
Styrene Content 34 - 38 %
34 - 38 %
Descriptive Properties Value Comments
Rigidity medium/high