Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® ELKONIUM 36 Silver Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer CMW Inc.
Trade Name ELKONIUM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONIUM 36 Silver Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The alloying of small amounts of one of the precious metals, platinum, palladium or gold with silver increases the hardness, and reduces the metal transfer tendency. These alloys maintain a low contact resistance during operation, as they are not susceptible to oxidation. They are susceptible to sulfide tarnishing however, to about the same degree as fine silver. They are suitable for contacts in sensitive devices in both AC and DC circuits.ELKONIUM® 36, a silver platinum alloy, and ELKONIUM® 45, a silver palladium alloy, both have low contact resistance comparable to fine silver. They are used in DC applications where contact forces are low and fine silver transfers excessively. ELKONIUM® 45 alloy is employed as a negative contact operating against a positive contact material such as ELKONIUM® 17, CMW® D55X (silver-cadmium oxide) or CMW® D510 (silver-nickel) alloys. These combinations are used in low voltage DC applications such as vibrating contact voltage regulators to minimize metal transfer.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.6 g/cc
0.383 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 45
45
annealed
77
77
cold worked
Tensile Strength, Ultimate 172 MPa
25000 psi
annealed
324 MPa
47000 psi
cold worked
Elongation at Break 3.0 %
3.0 %
cold worked
37 %
37 %
annealed
Component Elements Properties Metric English Comments
Platinum, Pt 3.0 %
3.0 %
Silver, Ag 97 %
97 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000380 ohm-cm
0.00000380 ohm-cm
45 % IACS
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved