Material Notes:
ELKONIUM® 28, a silver-manganese alloy, was developed by CMW specifically for the control of the transfer of contact material in low voltage DC applications. It is used as a positive contact operating against a CMW D582F (silver graphite, see Series 300) negative contact in vibrating contact automobile voltage regulators.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 11.0 g/cc
0.397 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 68
68
annealed
75
75
cold worked
Tensile Strength, Ultimate 207 MPa
30000 psi
annealed
276 MPa
40000 psi
cold worked
Elongation at Break 5.0 %
5.0 %
cold worked
32 %
32 %
annealed
Component Elements Properties Metric English Comments
Manganese, Mn 5.0 %
5.0 %
Silver, Ag 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000172 ohm-cm
0.0000172 ohm-cm
10 % IACS
Users viewing this material also viewed the following: