CMW® ELKONITE 30SB tungsten, silver

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Refractory Metal , Tungsten Alloy
Manufacturer CMW Inc.
Trade Name ELKONITE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE 30SB tungsten, silver.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 14.48 g/cc
0.5231 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 91
91
Component Elements Properties Metric English Comments
Silver, Ag 30 %
30 %
Tungsten, W 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000370 ohm-cm
0.00000370 ohm-cm
47 % IACS