CMW® DSC Copper with Dispersed Aluminum Oxide

Category Metal , Metal Matrix Composite , Nonferrous Metal , Copper Alloy
Manufacturer CMW Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® DSC Copper with Dispersed Aluminum Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CMW® DSC material is an extruded and cold worked powder metallurgy material consisting of copper and dispersed aluminum oxide. It has exceptional high temperature strength for its electrical conductivity both of which exceed the R.W.M.A Class 2 alloys.CMW® DSC is used to its best advantage when welding coated steels, such as galvanized, electo-coated, aluminized, terne plate. It's ability to resist deformation over a long period, make it a top choice for such applications particularly where extended production runs (without cap change) are required.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 75
75
Tensile Strength, Ultimate 372 MPa
54000 psi
Tensile Strength, Yield 345 MPa
50000 psi
Elongation at Break 25 %
25 %
Reduction of Area 80 %
80 %
Modulus of Elasticity 123 GPa
17800 ksi
Thermal Properties Metric English Comments
CTE, linear 19.0 µm/m-°C

@Temperature 100 °C
10.6 µin/in-°F

@Temperature 212 °F
Thermal Conductivity 345 W/m-K
2390 BTU-in/hr-ft²-°F
Melting Point 1080 °C
1980 °F
Softening Point 800 °C
1470 °F
Permanent Softening
Component Elements Properties Metric English Comments
Al2O3 0.50 %
0.50 %
Copper, Cu 99.5 %
99.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000203 ohm-cm
0.00000203 ohm-cm
85 % IACS