CIMBAR NANO-FLEX® Talc - D for TPO Applications

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name NANO-FLEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR NANO-FLEX® Talc - D for TPO Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NANO-FLEX® Talc is designed for use in high performance TPO applications that require high brightness and an high balance of stiffness and toughens. NANO-FLEX® Talc is made by a proprietary process that results in a very high aspect ratio, excellent dispersion and heat aging while offering excellent compounded color. NANO-FLEX® Talc-D, which can improve handling and initial compounding.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 2.80 g/cc
2.80 g/cc
Bulk Density 0.641 g/cc
0.0231 lb/in³
Loose
Brightness 70 %
70 %
wet
93 %
93 %
Hunter Y, Rd value, dry
Moisture Absorption at Equilibrium <= 0.50 %
<= 0.50 %
Loss On Ignition 7.0 %
7.0 %
Particle Size 0.70 µm
0.70 µm
D50
<= 2.7 µm
<= 2.7 µm
D98
Component Elements Properties Metric English Comments
Al2O3 <= 1.0 %
<= 1.0 %
CaO <= 1.0 %
<= 1.0 %
Fe2O3 <= 1.0 %
<= 1.0 %
MgO 30 %
30 %
SiO2 60 %
60 %