CIMBAR EliteTalc® 23 Cosmetic Talc

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name EliteTalc®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR EliteTalc® 23 Cosmetic Talc.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a moisture barrier, a dry lubricant, an excipient in medical applications and as a solid component in lotions. It can also be used in dusting applications where U.S.P. certified raw materials are required.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Bulk Density 0.593 g/cc
0.0214 lb/in³
Tapped
Brightness 90 %
90 %
"Rd", dry
Loss On Ignition 7.0 %
7.0 %
Particle Size 2.0 µm
2.0 µm
Median
Particle Mesh Size 325 Mesh
325 Mesh
0.5% retained
Component Elements Properties Metric English Comments
Al2O3 <= 1.0 %
<= 1.0 %
CaO <= 1.0 %
<= 1.0 %
Fe2O3 <= 1.0 %
<= 1.0 %
Lead, Pb <= 0.0010 %
<= 0.0010 %
MgO 31 %
31 %
SiO2 60 %
60 %