CENTROPLAST CENTROTRON GF 40 Polyphenylene sulfide 40% glass fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROTRON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROTRON GF 40 Polyphenylene sulfide 40% glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CENTROTRON GF is a plastic that is reinforced for high strength and rigidity, that can be used at high operating temperatures. Applications include bearings, sealing rings, rods and hollow bars. Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 185 MPa
26800 psi
v = 5 mm/min; ISO 527-2
Elongation at Break 1.9 %
1.9 %
ISO 527-2
Tensile Modulus 14.7 GPa
2130 ksi
ISO 527-2
Flexural Modulus 14.0 GPa
2030 ksi
ISO 178
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 210 °C
410 °F
Long Term
260 °C
500 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
ISO 75-2
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093