CENTROPLAST CENTROTRON GF 15 Polyphenylene sulfide 15% glass fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROTRON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROTRON GF 15 Polyphenylene sulfide 15% glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used in high temperature applications. CENTROTRON has a low sliding friction coefficient and high abrasion resistant. Applications include bearings, sealing rings, rods and hollow bars.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Water Absorption at Saturation 0.020 %
0.020 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 86.0 MPa
12500 psi
v = 5 mm/min; ISO 527-2
Elongation at Break 2.2 %
2.2 %
ISO 527-2
Tensile Modulus 5.00 GPa
725 ksi
ISO 527-2
Flexural Modulus 5.10 GPa
740 ksi
ISO 178
Charpy Impact Unnotched 4.80 J/cm²
22.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Long Term
240 °C
464 °F
Short term
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093