CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTRODAL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement of the friction and dry sliding behavior. Applications include bearing bushes, structural components subjected to dynamic loads, and sliding plates. Formerly Centrodal G.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.20 %
0.20 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.80 %
0.80 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 110 MPa
16000 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 43.0 MPa
6240 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 15 %
15 %
ISO 527-2
Tensile Modulus 2.20 GPa
319 ksi
ISO 527-2
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Coefficient of Friction, Dynamic 0.19
0.19
vs. steel
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Melting Point 166 °C
331 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 100 °C
212 °F
Long Term
140 °C
284 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
ISO 75-2
Vicat Softening Point 140 °C
284 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 6.00 mm
HB

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency 100 Hz
3.8

@Frequency 100 Hz
IEC 60250
3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
889 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0020

@Frequency 100 Hz
0.0020

@Frequency 100 Hz
IEC 60250
0.0070

@Frequency 1e+6 Hz
0.0070

@Frequency 1e+6 Hz
IEC 60250
Descriptive Properties Value Comments
Food Compliance yes
BGVV
yes
FD A
Copyright © lookpolymers.com All Rights Reserved