Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are microwave cookware and airline dishes.
Physical Properties Metric English Comments
Specific Gravity 1.70 - 2.10 g/cc
1.70 - 2.10 g/cc
Water Absorption 0.10 - 0.20 %
0.10 - 0.20 %
24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 65
45 - 65
Tensile Strength, Ultimate 34.5 - 55.2 MPa
5000 - 8000 psi
Flexural Strength 96.5 - 138 MPa
14000 - 20000 psi
Flexural Modulus 11.7 - 14.5 GPa
1700 - 2100 ksi
Compressive Strength 110 - 138 MPa
16000 - 20000 psi
Izod Impact, Notched 1.07 - 3.20 J/cm
2.00 - 6.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F