Buckeye Polymers BP PPC 0510 BLK Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP PPC 0510 BLK Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resistanceHigher melt flow available for improved processibilityProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Melt Flow 6.0 - 20 g/10 min
6.0 - 20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Izod Impact, Notched >= 0.801 J/cm
>= 1.50 ft-lb/in
ASTM D256
Gardner Impact >= 136 J
>= 100 ft-lb
ASTM D5420