Buckeye Polymers BP HDPE 9501 R BLK High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP HDPE 9501 R BLK High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: Our HDPE grade of materials are designed to offer excellent physical properties while providing cost savings versus higher cost prime equivalents. Buckeye Polymers HDPE materials are being used in many applications such as extruded lineals, and thermoformed applications.Product Features:Large volume availabilityISO 9001 approved quality and COA's with each shipmentMeets or exceeds GMP.PE.007Easily recyclable at point of moldingAppearance: BlackForms: PelletsProcessing Method: ExtrusionInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Density 0.950 - 0.955 g/cc
0.0343 - 0.0345 lb/in³
ASTM D1505
Melt Flow <= 1.0 g/10 min
<= 1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 22.1 MPa
>= 3200 psi
ASTM D638
Flexural Modulus >= 0.703 GPa
>= 102 ksi
ASTM D790
Izod Impact, Notched >= 2.14 J/cm
>= 4.00 ft-lb/in
ASTM D256
Gardner Impact >= 325 J
>= 240 ft-lb
ASTM D5420