Buckeye Polymers BP FLEX D6020 BLK Thermoplastic Polyolefin

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP FLEX D6020 BLK Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resistanceGood UV resistanceLow densityWide service range from -20°C to 120°CAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Melt Flow 14 - 20 g/10 min
14 - 20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62 - 68
62 - 68
ASTM D2240
Tensile Strength, Yield >= 16.0 MPa
>= 2320 psi
ASTM D638
Flexural Modulus >= 0.6998 GPa
>= 101.5 ksi
ASTM D790
Izod Impact, Notched >= 5.34 J/cm
>= 10.0 ft-lb/in
ASTM D256
Gardner Impact >= 407 J
>= 300 ft-lb
ASTM D5420