Material Notes:
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resistanceGood UV resistanceLow densityWide service range from -20°C to 120°CProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0080 - 0.018 cm/cm
0.0080 - 0.018 in/in
ASTM D955
Melt Flow 20 - 26 g/10 min
20 - 26 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 10.0 MPa
>= 1450 psi
ASTM D638
Flexural Modulus 0.379 - 0.7198 GPa
55.0 - 104.4 ksi
ASTM D790