Breplast Bretene SPM Thermoplastic Composite, 70% HD + 30% PP

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP)
Manufacturer Breplast S.P.A.
Trade Name Bretene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Breplast Bretene SPM Thermoplastic Composite, 70% HD + 30% PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A.
Physical Properties Metric English Comments
Density >= 0.945 g/cc
>= 0.0341 lb/in³
UNI EN ISO 1183-1
Melt Flow 1.5 - 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 - 3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
UNI EN ISO 1133
3.5 - 5.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 - 5.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
UNI EN ISO 1133
Descriptive Properties Value Comments
Color Dark Grey