Braskem TR3120C Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TR3120C Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Superior color and processing stability, low odor, good flow and set-up behavior, excellent see through clarity.Applications: Suggested uses include housewares, reusable food containers, packaging.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 29.6 MPa
4300 psi
2 in/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2 in/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256A