Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TR3020NT Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High flexural modulus, very good mold release. Applications: Suggested uses include extrusion, compression molding, thermoforming. Process: Compression Molding. This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 31.7 MPa
4600 psi
2 in/min; ASTM D638
Elongation at Yield 12 %
12 %
2 in/min; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
ASTM D256A