Description: Superior low temperature impact, nucleated, antistatic.Applications: Suggested uses include furniture, toys, compounding.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 19.3 MPa
2800 psi
2 in/min; ASTM D638
Elongation at Yield 5.5 %
5.5 %
2 in/min; ASTM D638
Flexural Modulus 0.931 GPa
135 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256A
Impact Test 40.7 J

@Temperature -29.0 °C
30.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Users viewing this material also viewed the following: