Material Notes:
Description: Good balance of stiffness and impact strength, excellent organoleptic properties.Applications: Suggested uses include compounding, thin-walled injection molding.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength 27.6 MPa
4000 psi
2 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
2 in/min; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256A