Material Notes:
Description: S1522 is a low density polyethylene produced in a high-pressure process, which presents good balance between mechanical properties and processability. Contain no additives.Applications: Blow molded articles for general purpose and injection blow molding.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM-D1505
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength at Break 12.0 MPa
1740 psi
ASTM-D638
Tensile Strength, Yield 11.0 MPa
1600 psi
ASTM-D638
Elongation at Break 850 %
850 %
ASTM D638
1% Secant Modulus 1.59 MPa
230 psi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
ASMT D3418
Vicat Softening Point 95.0 °C

@Load 1.02 kg
203 °F

@Load 2.25 lb
ASTM-D1525