Braskem PH 0950 HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PH 0950 HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PH 0950 is a medium melt flow rate homopolymer with an antiblocking agent. PH 0950 is specially designed for twisted films produced by cast or blown film extrusion. It exhibits excellent optical properties and good processability. It is used in twist film for sweets and candies.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM-D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM-D638
Elongation at Yield 9.0 %
9.0 %
ASTM-D638
Flexural Modulus, 1% Secant 1400 MPa
203000 psi
ASTM-D790
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
ASTM-D648
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
ASTM-D1525