Braskem PD 943XP HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PD 943XP HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PD 943XP is a medium melt flow rate homopolymer with slip and antiblocking agents. It is suitable for blown film extrusion. This product features good impact strength, excellent gloss and transparency, and good slipping and weldability. Its applications include: coil for automatic packaging, general purpose, and food and textile packaging.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM-D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM-D638
Elongation at Yield 11 %
11 %
ASTM-D638
Flexural Modulus, 1% Secant 1400 MPa
203000 psi
ASTM-D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM-D648
Vicat Softening Point 151 °C

@Load 1.02 kg
304 °F

@Load 2.25 lb
ASTM-D1525