Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem PCD 0140 HECO Polypropylene Heterophasic Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PCD 0140 HECO Polypropylene Heterophasic Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PCD 0140 is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140 is highly protected against thermal aging and designed for continuous use at high temperatures. Its applications include: undercoating, solid thermal coating, and foam thermal coating.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM-D792
Oxidative Induction Time (OIT) >= 50 min

@Temperature 220 °C
>= 50 min

@Temperature 428 °F
ASTM-D3895
Melt Flow 0.75 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.75 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM-D2240
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM-D638
Elongation at Break >= 400 %
>= 400 %
ASTM-D638
>= 140 %

@Time 1.26e+7 sec
>= 140 %

@Time 3500 hour
UV Stability; ASTM D155
Elongation at Yield 7.0 %
7.0 %
ASTM-D638
Flexural Modulus, 1% Secant 1100 MPa
160000 psi
ASTM-D790
Taber Abrasion, mg/1000 Cycles 7.0

@Load 1.00 kg
7.0

@Load 2.20 lb
CS-17; ASTM D4060
Thermal Properties Metric English Comments
Thermal Conductivity <= 0.220 W/m-K
<= 1.53 BTU-in/hr-ft²-°F
ASTM C177/C518
Melting Point 163 °C
325 °F
ASTM-D3418
Vicat Softening Point 146 °C

@Load 1.02 kg
295 °F

@Load 2.25 lb
ASTM-D1525
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM-D257
Users viewing this material also viewed the following: