Material Notes:
Injected lids and caps; Large flat surface injected pieces.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.923 g/cc
0.923 g/cc
ASTM D1505/D792
ESCR 10% Igepal® 3.0 hour

@Temperature 50.0 °C
3.0 hour

@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 42
42
ASTM D2240
Tensile Strength at Break 6.00 MPa
870 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Flexural Modulus, 1% Secant 700 MPa
102000 psi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525