Braskem PB 682 LDPE Blow Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PB 682 LDPE Blow Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PB682 is a low density polyethylene (LDPE), produced under high pressure technology. The end products molded with this resin present good dimensional stability and high flexibility.Applications: General bottles; cast film for diapers back sheets. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.0 MPa
1740 psi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 89.0 °C
192 °F
ASTM D1525